Payment Terms | L/C, T/T, Western Union, MoneyGram,paypal |
Supply Ability | 500kgs/month |
Delivery Time | 15-30days |
Packaging Details | Stardard export package |
Original Place | CHINA |
Packing | Standard wooden case |
Electrical Conductivity | 0.13 x 10^6 S/m |
Process | Mixing |
Port | Tianjin,Qingdao and Shanghai |
Product Standard | ASTM B 365-98 |
Conditions | Annealed |
Atomic Mass | 180.94788 g/mol |
Commodity | Tantalum tube |
Corrosion Resistance | outstanding |
Boiling Point | 5425°C |
Specifications | customized |
Application | electronics, chemicals |
Evaporation Heat | 743kJ/mol |
Shape | Crucible,as per drawing |
Brand Name | Changsheng |
Model Number | R05200 |
Certification | ISO 9001;2015 |
Place of Origin | China |
View Detail Information
Explore similar products
Tantalum Tube Price Per Kg For Aerospace Industry Chemical Industry
Tantalum Rod R05200 R05400 Tantalum Alloy Bar Ta10W Price Per Kg Chemical
Factory Hot Sell Titanium Alloy Folding Bike Frame Size 1.5mm And All Spare
Titanium Alloy Bike Frame For Mountain Bike Internal Wiring Internal Brake Shock
Product Specification
Payment Terms | L/C, T/T, Western Union, MoneyGram,paypal | Supply Ability | 500kgs/month |
Delivery Time | 15-30days | Packaging Details | Stardard export package |
Original Place | CHINA | Packing | Standard wooden case |
Electrical Conductivity | 0.13 x 10^6 S/m | Process | Mixing |
Port | Tianjin,Qingdao and Shanghai | Product Standard | ASTM B 365-98 |
Conditions | Annealed | Atomic Mass | 180.94788 g/mol |
Commodity | Tantalum tube | Corrosion Resistance | outstanding |
Boiling Point | 5425°C | Specifications | customized |
Application | electronics, chemicals | Evaporation Heat | 743kJ/mol |
Shape | Crucible,as per drawing | Brand Name | Changsheng |
Model Number | R05200 | Certification | ISO 9001;2015 |
Place of Origin | China | ||
High Light | Superalloy Tantalum Rods Bars ,Artificial Bone Implant Tantalum Rods Bars ,R05200 Tantalum Rods Bars |
Description
Tantalum rod is a rod shaped product made of tantalum tungsten alloy, The numbers are Ta1, Ta2. Implementation standard: ASTM B 365 GB/T26012-2010 or according to Beijing Oriental Color tantalum Niobium enterprise standard execution,the density of tantalum rod is usually greater than or equal to 16.6g/cm³, the supply state is polished surface, the size range can start from Φ0.15xL, can be customized according to customer requirements. Tantalum rods have high melting point (about 3000 degrees Celsius), good corrosion resistance, high density (about 16.6 g/cm ³) and other characteristics.
Product photo
Application
For the production of vacuum blast furnace heating parts, heat insulation parts and charging vessels, in the chemical industry can be used to make digesters, heaters,
Coolers, all kinds of utensils and devices, as well as in aviation, aerospace industry, medical equipment and other fields are widely used.
Chemical Composition
Grade | chemical composition %, max | |||||||||||
Fe | Si | Ni | W | Mo | Ti | Nb | O | C | H | N | Ta | |
Ta 1 | 0.005 | 0.005 | 0.005 | 0.005 | 0.002 | 0.002 | 0.005 | 0.02 | 0.004 | 0.002 | 0.005 | remain |
Ta 2 | 0.005 | 0.005 | 0.005 | 0.005 | 0.002 | 0.002 | 0.1 | 0.03 | 0.1 | 0.002 | 0.01 | remain |
FRQ
Commercial CE SAA ROHS Certificate Outdoor IP65 Waterproof 20W 30W 50W 100W 200W 12V LED Flood Lights
Q1. Can I have a sample order for led light?
A: Yes, we welcome sample order to test and check quality. Mixed samples are acceptable.
Q2. What about the lead time?
A: 3-5 days for Sample preparing ,8-10 working days for mass production.
Q3. Do you have any MOQ limit for led light order?
A: Low MOQ, 1pc for sample checking is available.
Q4. How do you ship the goods and how long does it take to arrive?
A: Ship by DHL, UPS, FedEx or TNT. It takes 3-5 days to arrive. Airline and sea shipping also optional.
Q5. How to proceed an order for led light?
A: Firstly let us know your requirements or application.
Secondly We quote according to your requirements or our suggestions.
Thirdly customer confirms the samples and places deposit for formal order.
Fourthly We arrange the production.
Q6. Is it OK to print my logo on led light product?
A: Yes. Please inform us formally before our production.
Q7: Do you offer guarantee for the products?
A: Yes, we offer 5 years warranty to our products.
Q8: How to deal with the faulty?
A: Firstly, Our products are produced in strict quality control system and the defective rate will be less than 0.2%.
Secondly, during the guarantee period, we will send new lights with new order for small quantity. For defective batch products, we will repair them and resend them to you or we can discuss the solution including re-call according to real situation.
Company Details
Business Type:
Manufacturer
Year Established:
2001
Total Annual:
3000000-4000000
Employee Number:
>100
Ecer Certification:
Verified Supplier
Baoji City Changsheng Titanium Co.,Ltd is registered in 2006. Registered capital of 10 million yuan, the legal person is Zhao Wenhua. Before 2006, the factory is formed as forged workshop, no been registered. The year of 2006 was exist as a starting for Changsheng Titanium Co. The factory is located... Baoji City Changsheng Titanium Co.,Ltd is registered in 2006. Registered capital of 10 million yuan, the legal person is Zhao Wenhua. Before 2006, the factory is formed as forged workshop, no been registered. The year of 2006 was exist as a starting for Changsheng Titanium Co. The factory is located...