Payment Terms | L/C, , T/T |
Delivery Time | 7 days |
Packaging Details | Ply-wooden Case /Iron Case/ Bundle with plastic Cap |
Product Name | Superalloy Pipe Flange |
Material | UNS N08020 Nickel Alloy 20 |
Process | Forged |
Flange Face | RF/FF/RTJ |
Brand Name | Yuhong |
Model Number | SB462 NO8020 |
Certification | ASTM B462 UNS N08020 Nickel Alloy 20 Superalloy Flange |
Place of Origin | China |
View Detail Information
Explore similar products
ASTM A182 F304/304L,F316/F316L Stainless Steel Flanges SORF / SOFF / WNRF Type
STAINLESS STEEL FLANGE,SORF,WNFF,DIN2573,A182, F304, 304L, 304H, SS316, 316L
ASTM B151 C70600 Copper Nickel Alloy Forged Flange SCH80 CL150 Weld Neck Rised
ASTM A105 Carbon Steel Forged Flange BLRF SORF WNRF Black Painted
Product Specification
Payment Terms | L/C, , T/T | Delivery Time | 7 days |
Packaging Details | Ply-wooden Case /Iron Case/ Bundle with plastic Cap | Product Name | Superalloy Pipe Flange |
Material | UNS N08020 Nickel Alloy 20 | Process | Forged |
Flange Face | RF/FF/RTJ | Brand Name | Yuhong |
Model Number | SB462 NO8020 | Certification | ASTM B462 UNS N08020 Nickel Alloy 20 Superalloy Flange |
Place of Origin | China | ||
High Light | Forged Nickel Alloy Flange ,Superalloy Pipe Flange N08020 ,Superalloy Nickel Alloy Flange |
ASTM B462 / ASME SB462 UNS N08020 Nickel Alloy 20 Superalloy Pipe Flange PT Available
We are one of the biggest projects pipeline products supplier in China, Our products contain steel pipe/tube,fittings, flanges. With development more than10 years, we have accumulated a great many clients all around the world and Yuhong products also won the great praise among the customers.
Alloy 20 will resist corrosion especially in those environments that contain chemicals like nitric acid, phosphoric acid, chlorides and sulfuric acid. Alloy 20 also has good mechanical properties at both ambient as well as elevated temperatures. Alloy 20 is often termed as a superalloy. ASTM B462/ ASME SB462 Uns N08020 Blind Flange has excellent resistance to general corrosion, pitting, and crevice corrosion in chemicals containing chlorides as well as in acidic medium or conditions that contain acidic solutions like sulfuric, phosphoric, and nitric acids.
Alloy 20 Forged and Plate Flange
ASTM B462 Alloy 20 Slip-On Flange | ASTM B462 Alloy 20 Threaded Flange |
ASTM B462 Alloy 20 Weld Neck Flange | ASTM B462 Alloy 20 Socket Weld Flange |
ASTM B462 Alloy 20 Blind Flange | ASTM B462 Alloy 20 Reducing Flange |
ASTM B462 Alloy 20 Lap Joint Flange | ASTM B462 Alloy 20 Plate Flange |
ASTM B462 Alloy 20 Orifice Flange | ASTM B462 Alloy 20 Forged Flange |
ASTM B462 Alloy 20 Ring Type Joint Flange | ASTM B462 Alloy 20 Square Flange |
Alloy 20 Flanges Equivalent Grades
STANDARD | WERKSTOFF NR. | UNS | AFNOR | EN |
Alloy 20 | 2.4660 | N08020 | Z2NCUD31-20AZ | NiCr20CuMo |
Mechanical Properties
Alloy | Tensile Strength, min. | Yield Strength, min. | Elongation, min. | Reduction of Area, min. | ||
---|---|---|---|---|---|---|
ASTM B462 | ksi | MPa | ksi | MPa | % | % |
UNS N08020 | 80 | 551 | 35 | 241 | 30.0 | 50.0 |
*All values shall be measured at room temperature.
*Alloy 20 flanges shall be supplied in stabilized-annealed condition.
Chemical Composition
Element | Wt, % |
---|---|
Carbon [C] | ≤0.07 |
Manganese [Mn] | ≤2.00 |
Phosphorus [P] | ≤0.045 |
Sulfur [S] | ≤0.035 |
Silicon [Si] | ≤1.00 |
Nickel [Ni] | 32.00~38.00 |
Chromium [Cr] | 19.00~21.00 |
Molybdenum [Mo] | 2.00~3.00 |
Copper [Cu] | 3.00~4.00 |
Niobium+Tantalum [Nb+Ta] | 8xCarbon~1 |
Iron | Remainder |
*The tabulated values are abstracted from ASTM B462 Gr. UNS N08020.
ASME SB462 Alloy 20 Slip on Flange Vs DIN 2.4660 Weld Neck Flange
The ASME SB462 Alloy 20 Slip on Flange is slipped into the pipe and then the connection is made with the help of double weld- one on the backside of the flange and one in the front. Generally, the slip on flanges are more affordable than the weld neck flanges, but it can become expensive with the number of welding and inspections. Also, the strength of the slip on flange under any internal pressure is around 2/3rd, and fatigue strength is around 1/3rd of that of the weld neck flange
The DIN 2.4660 Weld Neck Flange is easily recognizable by the tapered hub which comes from the bolted connection to the pipe. The connection is made here with the help of but twelding, and that helps in preventing any type of turbulence at the joint. It also minimizes erosion and reduces restriction in the product flow. The alloy 20 weld neck flanges offer enhanced strength under different types of environments.
Application
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Importer,Exporter,Trading Company,Seller,Other
Year Established:
2007
Total Annual:
50M-70M
Employee Number:
50~850
Ecer Certification:
Verified Supplier
YUHONG HOLDING GROUP is one of the largest Procurement, Engineering & Contracting Group companies in China. Our group branch company and factory have been already approved by : ABS, LR, DNV, GL, BV, CCS, KR, PED 97/23/EC, AD2000-WO, GOST9941-81, CCS, TS, CNNC, ISO9... YUHONG HOLDING GROUP is one of the largest Procurement, Engineering & Contracting Group companies in China. Our group branch company and factory have been already approved by : ABS, LR, DNV, GL, BV, CCS, KR, PED 97/23/EC, AD2000-WO, GOST9941-81, CCS, TS, CNNC, ISO9...
Get in touch with us
Leave a Message, we will call you back quickly!