Product Name | INCOLOY alloy 890 Alloy Round Bar |
Grades | INCOLOY alloy 890 |
Processing methods | Shot blasted,Peeled,Machined,etc |
Surface | Black,Rrough Turned,etc |
Profile | Round Bar,Forging Parts,etc |
Price Term | Ex-work,FOB etc. |
Brand Name | PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL |
Model Number | INCOLOY alloy 890 |
Certification | SGS,TUV,BV,ISO,MTC |
Place of Origin | China |
View Detail Information
Explore similar products
SAE 17-22-A Alloy Round Bar SAE J467b-1956 R1968 BH
17-22-AS Alloy Round Bar 17-22AS Special Purpose Alloys
X5CrNiCu15-5 Alloy Round Bar W-Nr 1.4545 Bar 15-5PH Steel
X33CrS16 Alloy Round Bar W-Nr 1.2085 Tool Steel
Product Specification
Payment Terms | T/T | Supply Ability | 100000KGS/Month |
Delivery Time | Ex-stock for delivery: 3-7 days Production lead time: 45-55days | Packaging Details | Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement |
Product Name | INCOLOY alloy 890 Alloy Round Bar | Grades | INCOLOY alloy 890 |
Processing methods | Shot blasted,Peeled,Machined,etc | Surface | Black,Rrough Turned,etc |
Profile | Round Bar,Forging Parts,etc | Price Term | Ex-work,FOB etc. |
Brand Name | PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL | Model Number | INCOLOY alloy 890 |
Certification | SGS,TUV,BV,ISO,MTC | Place of Origin | China |
High Light | high strength Alloy Round Bar ,INCOLOY alloy 890 Alloy Round Bar ,INCOLOY alloy 890 |
INCOLOY alloy 890 Alloy Round Bar 890 Superalloy Round Bar 890 Round Bar 890 Bar
Description
Our company provides INCOLOY alloy 890 Alloy Shot blasted Round Bar 890 Superalloy Ground Round Bar 890 Peeled Round Bar 890 Milled Bar.
All of INCOLOY alloy 890 Alloy Shot blasted Round Bar 890 Superalloy Ground Round Bar 890 Peeled Round Bar 890 Milled Bar conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.
Round bar / Wire rod (Diameter): 5.5mm to 800mm
Square bar / Flat bar: 3mm to 800mm
Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm
Products Details
INCOLOY alloy 890 Alloy Shot blasted Round Bar 890 Superalloy Ground Round Bar 890 Peeled Round Bar 890 Milled Bar.
Chemical Composition (weight%): | Mechanical Properties Under Final Heat Treatment: |
C (%): ≤ 0.10 Al (%): ≤0.70 Ti(%): ≤1.00 Fe(%): Remainder | Form: bar and rod Condition: cold worked and hot worked, annealed, at 1150 Deg. min. Tensile strength,σb/≥ MPa: 520 Yield strength, σ0.2/≥ MPa: 205 Elongation, δ ≥(%): 35.0 Reduction of area, ф ≥ (%): - Hardness | HRC: - Service temperature: above 593 Deg |
Applications:
INCOLOY alloy 890 Alloy Shot blasted Round Bar 890 Superalloy Ground Round Bar 890 Peeled Round Bar 890 Milled Bar.
Superalloy is widely used to produce the high temperature components for gas turbine in the field of aviation, naval vessels and industry:
Heat treating fixture
Furnace muffle
Nuclear reactor
Turbine engine parts - mechanical gears, gear shaft, main axis, blade
Mechanical parts - bolt and nut, fastener
Gas turbine,etc
INCOLOY alloy 890 Alloy Shot blasted Round Bar 890 Superalloy Ground Round Bar 890 Peeled Round Bar 890 Milled Bar.
FAQ
Q: How do you control the quality?
A: We have professional inspectors to analyze the chemical composition of INCOLOY alloy 890 Alloy Shot blasted Round Bar 890 Superalloy Ground Round Bar 890 Peeled Round Bar 890 Milled Bar. and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.
Q: Do you accept customization?
A: Yes. If you have special requirements for products or packaging, we can make them for you.
Q: Can you accept trial orders?
A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.
Q: How do I get samples?
A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Trading Company
Total Annual:
5000000-8000000
Employee Number:
10~30
Ecer Certification:
Active Member
Baoheng New Material is a specialty metals solutions center serving customers in a variety of industries, including Aerospace, Defense, Space, Fastener, Medical, Power Generation, Oil and Gas, Semiconductor and many others. Our business is based on un... Baoheng New Material is a specialty metals solutions center serving customers in a variety of industries, including Aerospace, Defense, Space, Fastener, Medical, Power Generation, Oil and Gas, Semiconductor and many others. Our business is based on un...
Get in touch with us
Leave a Message, we will call you back quickly!