Payment Terms | L/C, , T/T, Western Union, MoneyGram |
Supply Ability | 100 sets per month |
Delivery Time | 10 Days |
Packaging Details | Cartob Box |
Applied Standard | YDT757 |
Test Sample | Microwave tower |
Handle Material | Oak |
Hammer weight | 70g |
Hammer Mass | 210g±1g |
Hammer Material | 45 steel |
Hammer Hardness | Above HS40 |
Base Size | 250×250×15mm |
Brand Name | Sinuo |
Model Number | SN2209 |
Certification | Calibration Certificate (Cost Additional) |
Place of Origin | China |
View Detail Information
Explore similar products
100mm Drop Tester EN 71-1 Toys 1KG Impact Strength Test Apparatus
IEC60884-1 Switch Life Tester For Insulation Parts Thermal Resistance 20N Ball
Switches Intended for Self-ballasted Lamp Loads Automatic Breaking Capacity Test
Resistive Inductive Capacitive Load Cabinet for Switches Plugs and Sockets
Product Specification
Payment Terms | L/C, , T/T, Western Union, MoneyGram | Supply Ability | 100 sets per month |
Delivery Time | 10 Days | Packaging Details | Cartob Box |
Applied Standard | YDT757 | Test Sample | Microwave tower |
Handle Material | Oak | Hammer weight | 70g |
Hammer Mass | 210g±1g | Hammer Material | 45 steel |
Hammer Hardness | Above HS40 | Base Size | 250×250×15mm |
Brand Name | Sinuo | Model Number | SN2209 |
Certification | Calibration Certificate (Cost Additional) | Place of Origin | China |
High Light | Coating Adhesion Hammer Test Device ,Oak Handle Hammer Test Device ,Oak Handle Hammer Test Device |
YDT757 Galvanized Coating Adhesion Hammer Drop Test Device
Product Overview:
This test device conforms to the YDT757 drop hammer test method, and is suitable for hot-dip galvanized coating adhesion test. It uses a hammer to drop freely to hit the sample to test whether the galvanized coating meets the standard. This product is suitable for product quality inspection and control of similar iron tower manufacturers and quality inspection departments.
Sample and Restriction:
Transmission line tower, microwave tower.
Application:
It is used to test hot dip galvanized coating adhesion.
Test Principle:
Drop freely impact samples of the hammer head to test galvanized Layer meets standards or not.
Usage Instructions:
Adjust the device according to the countertop level to make it level, Adjust the sample so that the striking point is not less than 10mm away from the edge, corner, and end of the sample, the hammer head faces the center of the platform, the hammer handle is perpendicular to the base plane, and then falls freely, striking 5 points in parallel at 4mm intervals. Check whether the surface condition of the galvanized layer meets the requirements of the standard.
Technical Parameters:
Hammer weight | 210g±1g |
Hammer material | 45steel, |
Hammer hardness | Hardness above HS40 |
Vertical height from center line of hammer head to base surface | 300mm±1mm |
Hammer handle material | Oak |
Hammer handle mass | 70g |
Base plate | 250 ×250×15mm, equipped with horizontal level bubble |
Company Details
Business Type:
Manufacturer
Total Annual:
800000-1500000
Employee Number:
30~50
Ecer Certification:
Verified Supplier
Sinuo is an innovation manufacturing company, specializing in the research and development and sales of laboratory construction and testing equipment for electrical appliances (covering the construction of energy efficiency and performance laboratories, as well as supplementary waterproof testing la... Sinuo is an innovation manufacturing company, specializing in the research and development and sales of laboratory construction and testing equipment for electrical appliances (covering the construction of energy efficiency and performance laboratories, as well as supplementary waterproof testing la...
Get in touch with us
Leave a Message, we will call you back quickly!