Maximum Temperature | 1800℃ |
Thermal Conductivity | 18-25W/m·K |
Features | High temperature resistance, oxidation resistance, long service life |
Diameter | 3/6/9/12mm |
Length | 100/200/300/400/500/600/700/800/900/1000mm |
Material | Mosi2 |
Density | 6.5-7.5g/cm³ |
Surface Load | 6-12W/cm² |
Power | 100/200/300/400/500/600/700/800/900/1000W |
Usage | High temperature heating element for industrial furnaces |
Thermal Expansion Coefficient | 4.5-5.0×10^-6/K |
Maximum Bending Strength | 350MPa |
Voltage | 110/220/240V |
Shape | W shape |
Place of Origin | China |
Brand Name | SONGYU |
View Detail Information
Explore similar products
W Type Mosi2 Heating Element Molybdenum Disilicide Heating Elements
High Temperature MoSi2 Element 100mm-1000mm Moly Disilicide Heating Element
1800C Moly Disilicide Heating Elements MoSi2 Furnace Heating Element
SPK Moly Disilicide Heating Elements High Purity MoSi2 Heater
Product Specification
Payment Terms | T/T, Western Union | Supply Ability | Spark Industry (Henan) Co., Ltd. |
Delivery Time | 15 work days | Packaging Details | WOODEN CASE |
Maximum Temperature | 1800℃ | Thermal Conductivity | 18-25W/m·K |
Features | High temperature resistance, oxidation resistance, long service life | Diameter | 3/6/9/12mm |
Length | 100/200/300/400/500/600/700/800/900/1000mm | Material | Mosi2 |
Density | 6.5-7.5g/cm³ | Surface Load | 6-12W/cm² |
Power | 100/200/300/400/500/600/700/800/900/1000W | Usage | High temperature heating element for industrial furnaces |
Thermal Expansion Coefficient | 4.5-5.0×10^-6/K | Maximum Bending Strength | 350MPa |
Voltage | 110/220/240V | Shape | W shape |
Place of Origin | China | Brand Name | SONGYU |
High Light | W Type MoSi2 Element ,110V MoSi2 Element ,240V Moly Disilicide Heating Elements |
W type Mosi2 Heating Element
The standard specifications include:
1800: d x c: Various specifications including Φ 3/6, Φ 4/9, Φ 6/12, Φ 9/18, Φ 12/24, etc
Under high temperature oxidation atmosphere, a quartz protective layer is formed on the surface of the silicon molybdenum rod to prevent further oxidation. When the temperature of the component exceeds 1700 ℃, the quartz protective layer melts, and the component continues to be used in an oxidizing atmosphere, resulting in the regeneration of the quartz protective layer. Silicon molybdenum rods should not be used for a long time within the range of 400-700 ℃, otherwise the components will pulverize due to strong oxidation at low temperatures.
Atmosphere | SP1700 | SP1800 |
Air | 1700 | 1800 |
N2 Nitrogen | 1600 | 1700 |
Ar Ne Argon,Helium | 1600 | 1700 |
Dry Hydrogen(dew point)-80°C | 1150 | 1150 |
Wet Hydrogen(dew point)-20°C | 1450 | 1450 |
Exogas(e.g.10% CO2,50%CO,15%H2) | 1600 | 1700 |
Exogas(e.g.40%CO2,20%CO) | 1400 | 1450 |
Cracked and partially burnt ammonia | 1400 | 1450 |
Company Details
Business Type:
Manufacturer,Seller
Year Established:
2019
Total Annual:
>1000000
Employee Number:
50~100
Ecer Certification:
Verified Supplier
Zhengzhou Songyu High Temperature Technology Co., Ltd. is a comprehensive company specializing in the research and development, production, sales, and technical services of silicon carbide and molybdenum disilicide resistance heating elements. Adhere to customer-oriented approach and strive to conti... Zhengzhou Songyu High Temperature Technology Co., Ltd. is a comprehensive company specializing in the research and development, production, sales, and technical services of silicon carbide and molybdenum disilicide resistance heating elements. Adhere to customer-oriented approach and strive to conti...
Get in touch with us
Leave a Message, we will call you back quickly!