Supply Ability | 100TONS PER MONTH |
Delivery Time | 1-2MONTHS |
Packaging Details | EXPORT BAGS |
Material | Gold Leaching |
Product form | solid gray white block |
Leaching rate | (ore grade - leaching slag grade)/ore grade *100% |
Heap leaching process | 0.03-0.1% solution prepared with clean water for spraying |
Name | gold ore dressing agent |
Usage | Environmental Protection Gold Leaching Agent |
Type | Ore Dressing Equipment |
Warranty | 12 months |
Keyword | Metallic Ore Dressing Agent |
Model | Metallic Ore Dressing Agent |
Brand Name | ZTIC |
Model Number | Gold Leaching |
Certification | ISO, CE |
Place of Origin | Henan, China |
View Detail Information
Explore similar products
Low Failure Rate Sand Washing Equipment 20-180t/H 12 Months Warranty
Automated 1500mm Screw Bucket Wheel Sand Washer Machine Low Maintenance Rate
ISO 0.8-1.2rpm XS2600 Sand Washing Machine for mining Long Service Life
High Automation Reliability Ore Dressing Equipment Sand Washer Machine 200-300t
Product Specification
Supply Ability | 100TONS PER MONTH | Delivery Time | 1-2MONTHS |
Packaging Details | EXPORT BAGS | Material | Gold Leaching |
Product form | solid gray white block | Leaching rate | (ore grade - leaching slag grade)/ore grade *100% |
Heap leaching process | 0.03-0.1% solution prepared with clean water for spraying | Name | gold ore dressing agent |
Usage | Environmental Protection Gold Leaching Agent | Type | Ore Dressing Equipment |
Warranty | 12 months | Keyword | Metallic Ore Dressing Agent |
Model | Metallic Ore Dressing Agent | Brand Name | ZTIC |
Model Number | Gold Leaching | Certification | ISO, CE |
Place of Origin | Henan, China | ||
High Light | Gold Ore Dressing Agent ,Powder Gold Leaching Agent ,Ore Dressing Equipment Gold Leaching Agent |
Gold Recovery Chemical Removal Powder Gold Leaching Agent Of Ore Dressing Equipment
1. Gold Leaching Agent Of Ore Dressing Equipment Application scope;
(1) Applicable scope: gold, silver oxide ore, primary ore, cyanidation tail slag, sulfide ore, roasted gold concentrate, sulfuric acid slag, lead and zinc slag, anode mud, circuit board and other kinds of gold-containing materials;
(2) Applicable process: heap leaching, pool leaching, carbon pulp (stirring leaching) process.
2.Gold Leaching Agent Of Ore Dressing Equipment parameter
Product form | solid gray white block |
Dissolution method | It can be used after fully stirring and dissolving with water at room temperature |
Adjust basicity | lime or caustic soda is generally used to adjust and maintain PH value of 10-12 |
3.Gold Leaching Agent Of Ore Dressing Equipment Calculation of drug dispensing:
(1) Dosage can refer to the amount of sodium cyanide, it is recommended to conduct beneficiation test to determine the best use conditions. (According to experience: for 1-2g/t gold oxidized ore, the concentration of liquid is generally kept at 0.3-1‰, which can be adjusted appropriately according to different ore grade and impurity content)
(2) Method of use:
Heap leaching process: 0.03-0.1% solution prepared with clean water for spraying;
Stirring leaching process: it can be configured to add 10%-15% solution, or directly added to the stirring tank in the form of solid, the concentration of reagent in the leaching pulp is generally in the range of 0.03-0.1%.
(3) Calculation method of dosage:
Dosage of tonic = (optimal concentration value - current concentration value) × dosage of water;
It is assumed that the optimal concentration value is 0.8‰ (measured by water volume), the backwater concentration is 0.3‰, and the lean liquid pool is 1000 cubic meters of water. Dosage of tonic :(0.8-0.3) ×1000=800 kg
4. Gold extraction agent f Ore Dressing Equipment in the laboratory operation method:
(6) Immersion test (suitable for oxidized ore, primary ore, cyanide slag, sulfuric acid slag, gold concentrate, anode mud)
(7) Take 200-500 grams of comprehensive ore sample, grinding to -200 mesh accounted for about 85% by the ball mill (fineness does not need to grind), into the open (basin) container for use;
(8) Add water to soak, more than the mine surface 4-8 cm or so (according to the container size);
8. Adjust the PH value of basicity 11-12.
(9) Put in 0.2-2g of reagent, stir for 2 minutes and soak (before putting, break the reagent into powder and mix evenly, the specific dosage is determined according to the grade of precious metals and main elements in the mineral sample);
(10) Stir thoroughly every two to four hours, and measure the PH value after precipitation. The PH value of basicity is 11-12.
Sediment is required before sampling, clean water sample or leached slag is taken (the slag is filtered by a filter and then rinsed with water for more than 5 times);
The extraction rate was measured by sampling three times in a 12-hour, 24-hour and 36-hour process.
Leaching rate = (ore grade - leaching slag grade)/ore grade *100%
Gold Recovery Chemical Removal Powder Gold Leaching Agent Of Ore Dressing Equipment
Company Details
Business Type:
Manufacturer
Year Established:
1981
Total Annual:
80 million-100 million
Employee Number:
500~1000
Ecer Certification:
Verified Supplier
Luoyang Zhongtai Industries Co., Ltd. The company was founded in 1981 and finished joint stock reform in 2005. There are eight subsidiaries and it's an independent legal entity with the qualifications of operating import & export trade. With a garden-like industrial park and modern st... Luoyang Zhongtai Industries Co., Ltd. The company was founded in 1981 and finished joint stock reform in 2005. There are eight subsidiaries and it's an independent legal entity with the qualifications of operating import & export trade. With a garden-like industrial park and modern st...
Get in touch with us
Leave a Message, we will call you back quickly!