Payment Terms | Western Union, L/C, T/T |
Supply Ability | 300 Ton/Tons per Month |
Delivery Time | 25-30 days subject to the clients' requirement and quantity |
Packaging Details | packed and labeled according to the regulations and customer's requests.Great care is taken to avoid any damage which might otherwise be caused during storage or transportation. |
Standard | AISI, ASTM, BS, DIN, GB, JIS, Other,JIS,AISI,ASTM,GB,DIN,EN |
Grade | Hastelloy C276 |
Type | wire |
Special Use | Heat Exchanger |
Delivery | 25-30 days subject to the clients' requirements and quantity |
Price Term | Ex-Work,FOB,CNF,CFR,CIF,FCA,DDP,DDU |
Application | Industry |
Brand Name | BLM-HA-1 |
Place of Origin | Jiangsu, China (Mainland) |
View Detail Information
Explore similar products
AISI Standard Hastelloy Alloy , Hastelloy C276 Sheet For Chemical Processing
Hastelloy C276 Grade Hastelloy Alloy Bar With Outstanding Mechanical Properties
Prominent Corrosion Resistant Hastelloy Alloy Strip For Chemical Field
Corrosion Resistant Hastelloy C276 Forging , Hastelloy C276 Material GB Standard
Product Specification
Payment Terms | Western Union, L/C, T/T | Supply Ability | 300 Ton/Tons per Month |
Delivery Time | 25-30 days subject to the clients' requirement and quantity | Packaging Details | packed and labeled according to the regulations and customer's requests.Great care is taken to avoid any damage which might otherwise be caused during storage or transportation. |
Standard | AISI, ASTM, BS, DIN, GB, JIS, Other,JIS,AISI,ASTM,GB,DIN,EN | Grade | Hastelloy C276 |
Type | wire | Special Use | Heat Exchanger |
Delivery | 25-30 days subject to the clients' requirements and quantity | Price Term | Ex-Work,FOB,CNF,CFR,CIF,FCA,DDP,DDU |
Application | Industry | Brand Name | BLM-HA-1 |
Place of Origin | Jiangsu, China (Mainland) | ||
High Light | hastelloy c276 forging ,hastelloy c22 pipe |
Good price nickel alloy hastelloy c276 wire price
Chemical composition:
C | S | Mn | P | S | Ni | Cr | Mo | Fe | Co | W | V | |
Min | 14.5 | 15.0 | 4.0 | 3.0 | ||||||||
Max | 0.01 | 0.08 | 1.0 | 0.04 | 0.03 | Margin | 16.5 | 17.0 | 7.0 | 2.5 | 4.5 | 0.35 |
Hastelloy C-276 Physical properties:
Density | 8.9 g/cm³ |
Melting point | 1325-1370 ℃ |
Hastelloy C-276 alloy minimum mechanical properties in the room temperature
Alloy state | Tensile strength Rm N/mm² | Yield strength R P0. 2 N/mm² | Elongation A 5 % |
C /C276 | 690 | 283 | 40 |
Characteristic as below
1. Excellent corrosion resistance to most of corrosion media in oxidation and reduction environments.
2. Excellent resist pitting, crevice corrosion and stress corrosion cracking performance.
Hastelloy C-276 Metallurgical structure C276 is face-centered cubic lattice structure. Hastelloy C-276 Corrosion resistance C276 alloy suit for many kinds of chemical process industry which contain the oxidizing medium and reductant.
High molybdenum and chromium content make it can resist the chloride corrosion, and tungsten make it corrosion resistance better.
C276 is one of a few material that can resist the corrosion of most chlorine, hypochlorite and chlorine dioxide, this alloy have prominent corrosion resistance to high concentration chlorate( iron chloride and copper chloride).
Company Details
Business Type:
Manufacturer,Trading Company
Year Established:
2017
Total Annual:
1000000-3000000
Employee Number:
10~50
Ecer Certification:
Verified Supplier
Bloom(Suzhou) Materials Co., Ltd ,which located in the beautiful city of Zhangjiagang , Suzhou,China. Bloom Company is a technology research and development enterprises which integrats technology research and development, production and trade.It mainly dealing two types of products based on... Bloom(Suzhou) Materials Co., Ltd ,which located in the beautiful city of Zhangjiagang , Suzhou,China. Bloom Company is a technology research and development enterprises which integrats technology research and development, production and trade.It mainly dealing two types of products based on...
Get in touch with us
Leave a Message, we will call you back quickly!