China 317L S31703 1.4438 X2CrNiMo18-15/4 Higher Ductility, Stress Corrosion Resistance
China 317L S31703 1.4438 X2CrNiMo18-15/4 Higher Ductility, Stress Corrosion Resistance

  1. China 317L S31703 1.4438 X2CrNiMo18-15/4 Higher Ductility, Stress Corrosion Resistance
  2. China 317L S31703 1.4438 X2CrNiMo18-15/4 Higher Ductility, Stress Corrosion Resistance
  3. China 317L S31703 1.4438 X2CrNiMo18-15/4 Higher Ductility, Stress Corrosion Resistance
  4. China 317L S31703 1.4438 X2CrNiMo18-15/4 Higher Ductility, Stress Corrosion Resistance
  5. China 317L S31703 1.4438 X2CrNiMo18-15/4 Higher Ductility, Stress Corrosion Resistance

317L S31703 1.4438 X2CrNiMo18-15/4 Higher Ductility, Stress Corrosion Resistance

  1. MOQ: negotiation
  2. Price: Negotiation
  3. Get Latest Price
Payment Terms full payment by L/C or 20% down payment, balance before shipment
Delivery Time within 20 working days
Packaging Details Standard seaworth package
Grade: 316L
Standard: ASTM, EN, GB, JIS
Length: 1000-2000mm
Thickness: 0.3-3.0
Width: 1000-6000mm
Place of Origin: China
Technique: Cold Rolled
Surface: 2B or Polishing
Brand Name BAOSTEEL,TISCO,
Model Number 317L
Certification ISO
Place of Origin China

View Detail Information

Contact Now Ask for best deal
Get Latest Price Request a quote
  1. Product Details
  2. Company Details

Product Specification

Payment Terms full payment by L/C or 20% down payment, balance before shipment Delivery Time within 20 working days
Packaging Details Standard seaworth package Grade: 316L
Standard: ASTM, EN, GB, JIS Length: 1000-2000mm
Thickness: 0.3-3.0 Width: 1000-6000mm
Place of Origin: China Technique: Cold Rolled
Surface: 2B or Polishing Brand Name BAOSTEEL,TISCO,
Model Number 317L Certification ISO
Place of Origin China


Alloy 317L is a low-carbon, high molybdenum austenitic stainless steel with a higher nickel alloy content than 316L. Developed to resist the attack of sulfuric acid compounds, this alloy combines good corrosion resistance with excellent mechanical properties and ease of fabrication. These alloys are frequently used for flue gas desulfurization services in fossil-fuel power plants. Compared to other austenitic stainless steels, 317L offers a higher creep strength, stress to rupture, and tensile strength at elevated temperatures.

The higher molybdenum and chromium content of 317L provides excellent corrosion resistance compared to stainless steel grades like 304 or 316, and it resists phosphoric acid, sulfuric acid, and chloride pitting/crevice corrosion. The low carbon content of this grade of 317 also provides resistance to sensitization during welding, which allows it to maintain its corrosion resistance at grain boundaries and prevent intergranular stress corrosion cracking.

 

化学成分 物理性能
Chemical Composition(%) Physical Property
C Si Mn P S Cr Ni Ti N Cu Mo 屈服强度 Y.S. (Mpa) 抗拉强度 T.S( Mpa) 延伸率EL/% 硬度 HARDNESS
Min Min Min Min Min Min Min Min Min Min Min Min Min Min Min
          18.000 11.000       3.000 205 517 35.0  
Max Max Max Max Max Max Max Max Max Max Max Max Max Max Max
0.030 0.750 2.000 0.045 0.030 20.000 15.000   0.100   4.000       95 RB

 

Common Applications of 317L

  • Flue gas desulfurization systems found in fossil fuel plants
  • Chemical and Petrochemical Processing
  • Food and Beverage Processing
  • Power Generation — condensers
  • Pulp and Paper Processing
  • Textiles with acid dyes

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Trading Company,Seller,Other

  • Year Established:

    2017

  • Total Annual:

    20 Million-100 Million

  • Ecer Certification:

    Site Member

About Us   JUYE metal was established in 2017 and is located in Ningbo City,which is one of the China’s largest international port cities, with convenient transportation facilities and mature commercial service network for steel products. We are a fast-growing company, nearly a... About Us   JUYE metal was established in 2017 and is located in Ningbo City,which is one of the China’s largest international port cities, with convenient transportation facilities and mature commercial service network for steel products. We are a fast-growing company, nearly a...

+ Read More

Get in touch with us

  • Reach Us
  • Ningbo Juye Metal Technology co.,ltd
  • 1618-1620 Office ,Cnooc Mansion,No.316 Lingjiang Rd, Beilun, Ningbo, China
  • https://www.juyemetal.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement