Payment Terms | L/C, T/T, D/P, D/A |
Delivery Time | 1 |
Material | Nickel Alloy |
Application | Spring |
Brand Name | fushun |
Model Number | 902 |
Certification | ISO NQA |
Place of Origin | CHINA |
View Detail Information
Explore similar products
Nickel Alloy Spring Wire
Inconel 625, 2.4856, N06625, Nickel Alloy Spring Wire
Inconel 617, N06617, 2.4663 Nickel Alloy Spring Wire
Monel K500, N05500, 2.4375, Nickel Alloy Spring Wire
Product Specification
Payment Terms | L/C, T/T, D/P, D/A | Delivery Time | 1 |
Material | Nickel Alloy | Application | Spring |
Brand Name | fushun | Model Number | 902 |
Certification | ISO NQA | Place of Origin | CHINA |
A precipitation hardenable Nickel-Iron-Chromium alloy having outstanding controllable thermoelastic coefficient characteristics and excellent oxidation resistance in high temperature atmospheres. The alloy can be processed to have a constant modulus of elasticity at temperatures ranging from -45 to +65°C (-50 to +150°F).
Diameter: 0.1 - 40mm
Shape: round, square, flat, special shaped
Outstanding controllable thermoelastic coefficient characteristics.
Can be processed to have constant modulus of elasticity from from -45 to +65ºC (-50 to +150ºF).
Good for springs in watches and weighing equipment.
Age hardenable.
Springs in precise applications, such as
watches
weighing machines
UNS N09902
AWS 080
AMS 5225
AMS 5221
HS 261
Element | Min % | Max % |
C | – | 0.06 |
Mn | – | 0.8 |
Si | – | 1 |
P | – | 0.04 |
S | – | 0.04 |
Cr | 4.9 | 5.75 |
Ni+Co | 41 | 43.5 |
Ti | 2.2 | 2.75 |
Al | 0.3 | 0.8 |
Cr+(Ti-4xC) | 7.1 | 8.1 |
Co | – | 1 |
Fe | Bal | Bal |
Density | Melting Point | Coefficient of Expansion | Modulus of Rigidity | Modulus of Elasticity |
8.05 g/cm³ | 1480 °C | 7.6 μm/m °C (20 – 100 °C) | 62 – 69 kN/mm² | 165 – 200 kN/mm² |
0.291 lb/in³ | 2700 °F | 4.2 x 10-6 in/in °F (70 – 212 °F) | 8993 – 10008 ksi | 23932 – 29008 ksi |
Condition | Type | Temperature | Time | Cooling |
Spring Temper – For good all round properties | Age Harden | 650 °C (1200 °F) | 2 Hr | Air |
Spring Temper – For max stability | Stress Equalise Age Harden |
400 °C (750 °F) 650 °C (1200 °F) |
2 Hr 2 Hr |
Air Air |
Spring Temper – For minimum hysterisis & low thermoelastic coefficient | Stress Equalise | 400 °C (750 °F) | 2 Hr | Air |
Annealed | Approx. tensile strength | <800 N/mm² | <116 ksi |
Approx. operating temperature (for constant modulus applications) | -45 to +65 °C | -50 to +150 °F | |
Spring Tempered | Approx. tensile strength | 900 – 1100 N/mm² | 131 – 159 ksi |
Approx. operating temperature (for constant modulus applications) | -45 to +65 °C | -50 to +150 °F | |
Spring Temper + Aged | Approx. tensile strength | 1300 – 1500 N/mm² | 189 – 218 ksi |
Approx. operating temperature (for constant modulus applications) | -45 to +65 °C | -50 to +150 °F |
Company Details
Business Type:
Manufacturer
Year Established:
1998
Total Annual:
10 millon-100 millon
Employee Number:
50~99
Ecer Certification:
Site Member
For over 20 years, Fushun Steel, have been dedicated to manufacturing high-quality spring steel wire. Our stable quality and superior technique are the foundations of our success, and we pride ourselves on delivering products that meet or exceed our customers' expectations. With a focus on innov... For over 20 years, Fushun Steel, have been dedicated to manufacturing high-quality spring steel wire. Our stable quality and superior technique are the foundations of our success, and we pride ourselves on delivering products that meet or exceed our customers' expectations. With a focus on innov...
Get in touch with us