Payment Terms | L/C, D/A, D/P, Western Union, |
Supply Ability | 5 Set/Sets per Year |
Delivery Time | 120 days |
Packaging Details | Standard export wooden cases and container |
Brand Name | Easy Fashion |
Certification | CE,CB,CQC,FC |
Place of Origin | Hunan, China(Mainland) |
View Detail Information
Explore similar products
Atomizing Molten Iron Powder Manufacturing Process , Equipment Needed For Powder
Atomization Chamber Gas Atomization Equipment 10m X 10m X 12m Dimension
Safe Gas Atomization Equipment Fit Double Crucible Melting Furnace Metal Powder
High Pressure Gas Atomization Equipment 100 ~ 500 Ppm Oxygen Content
Product Specification
Payment Terms | L/C, D/A, D/P, Western Union, | Supply Ability | 5 Set/Sets per Year |
Delivery Time | 120 days | Packaging Details | Standard export wooden cases and container |
Brand Name | Easy Fashion | Certification | CE,CB,CQC,FC |
Place of Origin | Hunan, China(Mainland) | ||
High Light | aluminum powder making machine ,gas atomization powder manufacturing equipment |
Plasma Rotate Electrode Process(PREP)
Overview
Metal or alloy are made into consumable electrodes as feedstock. Its end face is heated by plasma torch and melt into molten liquid, then the molten is ejected by the centrifugal force of high-speed rotating electrode, crushed into small droplets and solidified into powders. Helium is the best choice as protective atmosphere because its thermal conductivity is highest and alsmost 10 times of Ar. By using helium, cooling speed can be increased and plasma torch performance can be improved.
Schematic Diagram
This equipment is used for producing superalloy powders of 50-500 micron which are applied as materials for high temperature rotating components of turbine disc of aero engine, compressor disc, etc and for energy conversion devices of aerospace craft, nuclear reactor, petrochemical equipment, and coal conversion etc.
Features
TC4 Powders SEM, PREP(left) and GA(right)
It used for producing high melting and alive metal powders, such as nickel-based or Ti-based alloy powder. It’s also suitable for producing various alloy powders, such as steel, cobalt, chromium, etc.
The feedstock doesn’t contact with refractory materials during melting and atomizing processes, which eliminates non-metallic inclusions of pollution sources and produces clean powders.
The atomized powders is of regular shape, high sphericity, bright surface and good fluidity.
There’s no satellite phenomenon and hollow powder.
Powder particle distribution.
Manufacturing numerous special alloy powders as fast solidification overcomes aliquation.
Specifications
Total power: 150kw-200kw
Feedstock size: (φ45-φ75)×500mm
Feeding method: rod raw continuous feeding; max. rotation speed 15000-16000r/min.
Powder size: D50=100-150μm
Powder quality: sphericity rate over 90%; oxygen content under 300ppm.
Gas consumption: pure Ar.
Capacity: 40~150/8hour.
Company Details
Business Type:
Manufacturer,Importer,Exporter,Seller
Year Established:
2008
Total Annual:
7000000-12000000
Employee Number:
100~150
Ecer Certification:
Active Member
EasyFashion is the multifaceted supplier of Atomization Powder Manufacturing Equipment, Cemented Carbide Equipment and Heat Treatment Equipment being in 2008. We are most proud of our professional R & D team, experienced sales and after-sales team, for different materials in various areas of hea... EasyFashion is the multifaceted supplier of Atomization Powder Manufacturing Equipment, Cemented Carbide Equipment and Heat Treatment Equipment being in 2008. We are most proud of our professional R & D team, experienced sales and after-sales team, for different materials in various areas of hea...
Get in touch with us
Leave a Message, we will call you back quickly!