China factories

China factory - Wuxi Jinlai Mechanical Processing Co., Ltd.

Wuxi Jinlai Mechanical Processing Co., Ltd.

  • China,Wuxi ,Jiangsu
  • Active Member

Leave a Message

we will call you back quickly!

Submit Requirement
China 50-75mm Casting Superalloy Nicke Basedl Alloy round bars for Industry
China 50-75mm Casting Superalloy Nicke Basedl Alloy round bars for Industry

  1. China 50-75mm Casting Superalloy Nicke Basedl Alloy round bars for Industry
  2. China 50-75mm Casting Superalloy Nicke Basedl Alloy round bars for Industry
  3. China 50-75mm Casting Superalloy Nicke Basedl Alloy round bars for Industry

50-75mm Casting Superalloy Nicke Basedl Alloy round bars for Industry

  1. MOQ: 3 tons
  2. Price: Negotiable based on the quantity
  3. Get Latest Price
Payment Terms T/T, Western Union, L/C
Supply Ability 6000 tons per month
Delivery Time 30-60 days
Packaging Details Standard seaport packing or as custom request
Grade Nickle
Standard AISI, ASTM, BS, DIN, GB, JIS
Diameter 50-75 mm
Ni (Min): 57%
Ultimate Strength (≥ MPa): 900
Elongation (≥ %): 30
Application: Industry
Port Shanghai
Brand Name Wuxi Jinlai
Model Number Nickle Bar
Certification ISO
Place of Origin CHINA

View Detail Information

Contact Now Ask for best deal
Get Latest Price Request a quote
  1. Product Details
  2. Company Details

Product Specification

Payment Terms T/T, Western Union, L/C Supply Ability 6000 tons per month
Delivery Time 30-60 days Packaging Details Standard seaport packing or as custom request
Grade Nickle Standard AISI, ASTM, BS, DIN, GB, JIS
Diameter 50-75 mm Ni (Min): 57%
Ultimate Strength (≥ MPa): 900 Elongation (≥ %): 30
Application: Industry Port Shanghai
Brand Name Wuxi Jinlai Model Number Nickle Bar
Certification ISO Place of Origin CHINA

Casting Superalloy Nicke Basedl Alloy Mar-M246 In713c Inconel718 C276

Product Name
High temperature nickel based alloy powder Hastelloy C-22 Inconel 718 Inconel 713C
Material
Monel/Inconel/Hastelloy/Duplex Steel/PH Steel/Nickel Alloy
Shape
Round,Forging,Ring,Coil,Flange,Disc,Foil,Spherical,Ribbon,Square,Bar,Pipe,Sheet
Grade
Alloy:alloy 20/28/31
Hastelloy:Hastelloy B/-2/B-3/C22/C-4/S/C276/C-2000/G-35/G-30/X/N/g;
Hastelloy B/UNS N10001.hastelloy B-2/UNS N10665/
DIN W.Nr 2.4617,Hastelloy C,HastelloyC-4/UNS N06455/DIN W.Nr,2.4610,HastelloyC-22/UNS N06022/DIN W.Nr.2.4602,Hastelloy X/UNS N0602/DIN W.Nr.2.4665
Haynes:Haynes 230/556/188;
Inconel Series:
Inconel 600/601/602CA/617/625/713/718/738
Inconel 718/uns n07718/
Incoloy:incoloy 800/800H/800HT/825/925/926
GH:GH2132,GH3030,GH3039,GH3128;GH4180;GH3044
Monel:Monel 400/K50/R405
Nitronic:Nitronic 40/50/60
Nimonic :Nimonic 75/80A/90A/A263
Specification
Wire:0.01-10mm
Strip:0.05*5.0-5.0*250mm
Bar:dia4-50mm,length 2000-5000mm
Pipe
Product Characteristics
1.According to the preparation process can be divided into deformation superalloys.casting superalloys and power metallurgy superalloys.
2.According to the strengthening mode,there are solid solution strengthening type,precipitation strengthening type,oxide dispersion strengthening type and fober strengthening type,etc...
Standard
GB,AISI,ASTM,DIN,EN,SUS,UNS etc.
Inspection
ISO,SGS,BV AND SO ON.
Application
High temperature components such as turbing blades,guide vanes ,turbine disks,high pressure compressor disks,machine manufacturing
Packaging
1.cases packed in wooden cases
2.paper packaging
3.plastic packing
4.foam packaging
Packaging according to customer requirements or products
Delivery
7-25 days or according to the products
 
                                                          
 
Nickel-Based Alloys
Nickel-based alloys are alloys with high strength and corrosion resistance at 650-1000℃.According to its main properties,it is subdivided into nickel-based heat resistant alloy,nickel-based corrosion resistant alloy,nickel-based wear resistant alloy,nickel-based precision alloy and nickel-based shape mempry alloy.According to the matrix,the superalloy is divided into:iron base superalloy,nickel base superalloy and cobalt base superalloy.Nickel-based superalloy is referred to as nickel -based alloy.
 
Representative materials of nickel-based alloys are:
1.Incoloy alloys,such as Incoloy800,are mainly composed of :32Ni-Cr-21Ti,Al;Belongs to heat resistant alloy;
2.Inconel alloys,such as Inconel600,are mainly composed of:Ni-Cr- 15-73 Ti,Al;Belongs to heat resistant alloy;
3.Hastelloy alloy,namely Hastelloy alloy,such as Hastelloy c-276,is mainly composed of :56Ni-Cr-16 of 16 Mo-4W;
Belongs to corrosion resistant alloy.
4.Monel alloys,Monel alloys,such as Monel 400,are mainly composed of:34Cu Ni-65;Belongs to corrosion resistant alloy;
 

 
 
If you have any question, please feel free to contact us any time.



Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Agent,Exporter,Trading Company,Seller

  • Year Established:

    2008

  • Total Annual:

    10000000-20000000

  • Employee Number:

    100~200

  • Ecer Certification:

    Active Member

   Wuxi Jinlai Machinery Processing co. LTD has been engaged in steel industry for more than 12 years. We are famous in our country with good reputation, high-quality products, solid strength and lower price. Our products include carbon steel, wear resistant plate , galvanized steel p...    Wuxi Jinlai Machinery Processing co. LTD has been engaged in steel industry for more than 12 years. We are famous in our country with good reputation, high-quality products, solid strength and lower price. Our products include carbon steel, wear resistant plate , galvanized steel p...

+ Read More

Get in touch with us

  • Reach Us
  • Wuxi Jinlai Mechanical Processing Co., Ltd.
  • NO.21 Dongting Road,Xishan District,Wuxi ,Jiangsu,China
  • http://www.carbonsteelsheet.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement