Payment Terms | T/T, L/C, Western Union, MoneyGram, D/A, D/P |
Supply Ability | 20 sets per month |
Delivery Time | 5~10 work days |
Packaging Details | Carton |
Product name | Calorimeter DSC Plastic Differential Scanning Calorimetry Price |
Model | DSC-1150B |
DSC range | 0~±500 mw |
Temperature range | RT ~1150℃ |
Aluminum crucibles | Φ6.6*3mm (Diameter * High) |
Ceramic crucibles | Φ6.6*3mm (Diameter*High) |
Customized support | OEM, ODM |
Brand Name | JINHAIHU |
Model Number | DSC-1150B |
Certification | ISO |
Place of Origin | BEIJING, CHINA |
View Detail Information
Explore similar products
Plastics 500mW Dsc Differential Scanning Calorimetry Machine
Determination Glass Transition Temperature Differential Scanning Calorimetry
0.1mW Oxidation Induction Time Test Machine For Plastic Analysis
Melting Crystallization Temperature Enthalpy ISO Heat Measure Instrument
Product Specification
Payment Terms | T/T, L/C, Western Union, MoneyGram, D/A, D/P | Supply Ability | 20 sets per month |
Delivery Time | 5~10 work days | Packaging Details | Carton |
Product name | Calorimeter DSC Plastic Differential Scanning Calorimetry Price | Model | DSC-1150B |
DSC range | 0~±500 mw | Temperature range | RT ~1150℃ |
Aluminum crucibles | Φ6.6*3mm (Diameter * High) | Ceramic crucibles | Φ6.6*3mm (Diameter*High) |
Customized support | OEM, ODM | Brand Name | JINHAIHU |
Model Number | DSC-1150B | Certification | ISO |
Place of Origin | BEIJING, CHINA | ||
High Light | plastic dsc differential scanning calorimetry ,calorimeter dsc differential scanning calorimetry ,500mw dsc differential scanning calorimetry |
Melting and crystallization temperature and enthalpy measuring instrument
Application:
The instrument features:
Temperature range | RT-1150℃ |
Temperature resolution | 0.01℃ |
Heating rate | 0.1~80℃/min |
Constant temperature | RT-1150℃ |
Duration of constant temperature | The constant temperature time is unlimited at low temperature; When more than 1000 ℃, it is recommended that a single constant temperature time is less than 30 min |
Temperature control mode | Heating, cooling, constant temperature, any combination of three modes cycle use, temperature uninterrupted |
DSC range | 0~±500mW |
DSC resolution | 0.01mW |
DSC sensitivity | 0.01mW |
Working power | AC 220V 50Hz 300W or other |
Atmosphere control gas | Two-channel gas control by automatic controlled (e.g. nitrogen and oxygen) |
Gas flow | 0-200mL/min |
Gas pressure | 0.2MPa |
Gas flow accuracy | 0.2mL/min |
Crucible | Aluminium crucible Φ6.6*3mm (Diameter * High),ceramic crucible Φ6.6*3mm (Diameter * High) |
Calibration standard | With standard material (Indium, tin, zinc, silver), users can adjust the temperature coefficient and enthalpy value coefficient by themselves |
Data interface | Standard USB interface |
Display mode | 7-inch touch screen |
Output mode | computer and printer |
Design features | Fully closed support structure design, prevent items falling into the furnace body, pollution of the furnace body, reduce the maintenance rate |
Company Details
Business Type:
Manufacturer,Seller
Year Established:
2013
Employee Number:
50~100
Ecer Certification:
Verified Supplier
Beijing Jinshengxin testing machine Co., Ltd, covering 20,000 square meters, is located in Jinhaihu Town of Beijing. Since founded in 2003, our company has been devoted to the research, development and manufacture of testing machines for metallic and non-metallic materials, especially b... Beijing Jinshengxin testing machine Co., Ltd, covering 20,000 square meters, is located in Jinhaihu Town of Beijing. Since founded in 2003, our company has been devoted to the research, development and manufacture of testing machines for metallic and non-metallic materials, especially b...
Get in touch with us
Leave a Message, we will call you back quickly!