Delivery Time | 60-90DAYS |
Packaging Details | steel box/pallet |
Material | Aluminium, Carbon steel, Copper, Titanium |
Application | Engineering for oil&gas, chemical industry |
Process | explosive bonding and hot rolled |
Brand Name | RUISEN |
Place of Origin | CHINA |
View Detail Information
Explore similar products
Aluminium Titanium Copper Clad Plates Potroom Cathode For Alumnum Smelter
Cathode Crimper Explosive Welding Process Aluminum Copper High Efficiency
Trimetallic Explosion Bonded Clad Plate Wear Resistant For Anode Assembly
Cathode Aluminum Soft Tape Copper Crimper Welding For Reduction Cell
Product Specification
Delivery Time | 60-90DAYS | Packaging Details | steel box/pallet |
Material | Aluminium, Carbon steel, Copper, Titanium | Application | Engineering for oil&gas, chemical industry |
Process | explosive bonding and hot rolled | Brand Name | RUISEN |
Place of Origin | CHINA | ||
High Light | Aluminium Steel Explosive Clad Plate ,Potroom Explosive Clad Plate ,Aluminum Smelter Clad Plate |
Explosive welding Clad metals are a low-resistance, high-strength joint that allows the welding of two dissimilar metals. They are for use in high-current, high-temperature, and mechanical stress environments.
In the potroom, steel anode yokes are pre-welded to the aluminium anode rods using a bimetallic or trimetallic clads. This anode clad is a preformed aluminium/steel joint allowing the welding of the aluminium rod to the steel yoke, and forms a low-resistance, high-strength joint to withstand the elevated temperatures, mechanical abuse, and high current density found in the process.
Advantages
1. Electrical
The electrical resistance of a transition insert is nominally the series resistance of the components. There is no resistance increase or electrical conductivity loss associated solely with the bond or bonding process.
2. Strength
The technology is tensile tested at the bond to exceed the strength of the aluminium. High purity aluminium is typically 85-90 MPa in tensile strength, while the Pyrotek roll-bonded transition insert demonstrates a bond tensile strength of greater than 125 MPa as-rolled.
3.Temperature
Aluminium steel inserts can operate safely at elevated temperatures. The parts have been tested per SOHAR qualifying tests. For the 20°C Tensile test, clads always meet the 150MPa minimum requirement, often exceeding 180MPa. At 500°C , the minimum requirement is 85MPa, Pyrotek clads typically exceed 120MPa. Clads with no interlayer can withstand consistent temperatures up to 400°C. Adding a Titanium interlayer allows for operating temperatures up to 500°C.
Potroom Explosive welding anode clads
-Aluminium Steel explosive welding;
AL1050/1060+Q235B(1008)
Size: 12+40mm*175*175mm
12+40mm*185*185mm
based on yr drawing requests.
Company Details
Business Type:
Manufacturer,Exporter
Year Established:
1997
Total Annual:
1,000,000-12,000,000
Employee Number:
250~300
Ecer Certification:
Verified Supplier
Shaanxi Ruisen Metallic Composite Material Co., Ltd (Xian Ruisen Clad Metal Material Co., Ltd., in 1997) was established in 2018, with a registered capital of 100 million yuan, covering an area of 84 acres, including 36,000 square meters of workshops.With a number of patented technologies, is s... Shaanxi Ruisen Metallic Composite Material Co., Ltd (Xian Ruisen Clad Metal Material Co., Ltd., in 1997) was established in 2018, with a registered capital of 100 million yuan, covering an area of 84 acres, including 36,000 square meters of workshops.With a number of patented technologies, is s...