Payment Terms | L/C, T/T, Western Union |
Delivery Time | 20days |
Packaging Details | plastic bag+carton+wood pallet |
Material | carbon steel , stainless steel |
Size | M6-M52 |
Surface | Zinc plated, HDG,Yellow |
Port | Shanghai, Ningbo, Zhapu |
Garde | 4.8,8.8,10.9,SS304,SS316 |
Standard | DIN,ISO,ANSI,GB,ASTM |
Packing | Bags,small box package,suit for shipping or according to requirement,small plain box,Bulk Carton |
Type | Flat Washer,Mechanical Parts,Flat Gasket,Hardware Fasteners |
Model Number | M16 |
Place of Origin | CHINA |
View Detail Information
Explore similar products
Decorative Thin Steel Square Flat Washers Hardware Fasteners Type Widely Use
Plain Square Strut Washer Hot Dip Galvanized Reduce Friction 4.8 6.8 Grade
Ring Gasket Square Flat Washers Prevent Loosening For Electrical Applications
Large Diameter Stainless Steel Washers Zinc Plated High Precison Hardware
Product Specification
Payment Terms | L/C, T/T, Western Union | Delivery Time | 20days |
Packaging Details | plastic bag+carton+wood pallet | Material | carbon steel , stainless steel |
Size | M6-M52 | Surface | Zinc plated, HDG,Yellow |
Port | Shanghai, Ningbo, Zhapu | Garde | 4.8,8.8,10.9,SS304,SS316 |
Standard | DIN,ISO,ANSI,GB,ASTM | Packing | Bags,small box package,suit for shipping or according to requirement,small plain box,Bulk Carton |
Type | Flat Washer,Mechanical Parts,Flat Gasket,Hardware Fasteners | Model Number | M16 |
Place of Origin | CHINA | ||
High Light | thick steel washers ,square metal washers |
High Quality DIN436-1990 Zinc Plated With Round Hole Square Flat Washers M8,M10,M12
Product Description:
A washer is a thin plate with a hole typically in the middle that is normally used to distribute the load of a threaded fastener, such as a screw or nut. Other uses are as a spacer, spring wave washer, preload indicating device, locking device, and to reduce vibration. Washers usually have an outer diameter about twice larger than their inner diameter. Washers are usually stainless steel or carbon steel or plastic. High-quality joints require hardened steel washers to prevent the loss of pre-load due to the torque is applied
A washer is a thin plate (typically disk-shaped) with a hole (typically in the middle) that is normally used to distribute the load of a threaded fastener, such as a bolt or nut. Other uses are as a spacer, spring (Belleville washer, wave washer), wear pad, preload indicating device, locking device, and to reduce vibration (rubber washer). Washers often have an outer diameter (OD) about twice their inner diameter (ID), but this can vary quite widely.
Washers are usually metal or plastic. High-quality bolted joints require hardened steel washers to prevent the loss of pre-load due to Brinelling after the torque is applied.
Rubber or fiber gaskets used in taps (or faucets, or valves) to stop the flow of water are sometimes referred to colloquially as washers; but, while they may look similar, washers and gaskets are usually designed for different functions and made differently.
Washers are also important for preventing galvanic corrosion, particularly by insulating steel screws from aluminum surfaces.
Specification:
1. Material: Low Carbon steel, Mild Carbon steel, Stainless steel
2. Dimension: M3-M52, 3/16-24---2”
3. Grade: 4.8, 5.8, 6.8, 8.8, B7, 10.9
4. Coating: Plain, Black, Zinc Plated, HDG
5. Packing: Nylon bag, Carton ,pallet
6. Standard: DIN, ASTM/UNC,BSW,ISO,GB
7. Delivery: at least 20days
8. Port: Shanghai, Ningbo, Zhapu
9. Payment Terms: T/T, L/C
10. Name: High Quality DIN436-1990 Zinc Plated With Round Hole Square Flat Washers M8,M10,M12
Size | A | B | T | |||
Max. | Min. | Max. | Min. | Max. | Min. | |
5 | 5.80 | 5.5 | 18 | 16.9 | 2.3 | 1.7 |
6 | 6.96 | 6.6 | 22 | 20.7 | 2.3 | 1.7 |
8 | 9.36 | 9 | 28 | 26.7 | 3.6 | 2.4 |
10 | 11.43 | 11 | 34 | 32.4 | 3.6 | 2.4 |
12 | 13.93 | 13.5 | 44 | 42.4 | 4.6 | 3.4 |
14 | 15.93 | 15.5 | 50 | 48.4 | 4.6 | 3.6 |
16 | 18.2 | 17.5 | 56 | 54.1 | 6 | 4 |
20 | 22.84 | 22 | 72 | 70.1 | 7 | 5 |
22 | 24.84 | 24 | 80 | 78.1 | 7 | 5 |
24 | 28.84 | 26 | 85 | 82.8 | 7 | 5 |
27 | 30.84 | 30 | 98 | 95.88 | 7 | 5 |
30 | 34 | 33 | 105 | 102.8 | 7 | 5 |
33 | 37 | 36 | 112 | 109.8 | 7 | 5 |
36 | 40 | 39 | 125 | 122.5 | 9.2 | 6.8 |
39 | 43 | 42 | 140 | 137.5 | 9.2 | 6.8 |
42 | 46 | 45 | 150 | 147.5 | 9.2 | 6.8 |
45 | 49 | 48 | 160 | 157.5 | 9.2 | 6.8 |
48 | 63.2 | 52 | 170 | 167.5 | 11.2 | 8.8 |
Application:
Flat washer, also known as plain washer, mainly iron plates punched out, the general shape of a flat washer, a hole in the middle. The pore size specifications according to customer requirements are generally given. Flat washers generally thin pieces of various shapes, to reduce friction, prevent leakage, isolate, prevent loosening or dispersed pressure. Flat washers are mainly used to reduce the pressure, when some parts of the tightening axial force is large, easy to make dish washer pressed into, and then would be able to increase the hardness of the material to resolve. Many materials and structures have this part, for the performance of all kinds of similar effect.
Bearing surface by a threaded fastener material and process limitations, bolts and other fasteners little, so as to reduce the stress bearing surfaces protect the connector surface, which employs a gasket. Flat washers which spread a load and prevent damage to the surface being fixed. Actually , a flat washer may be used when the hole is a larger diameter than the fixing nut. A flat washer with a large outer diameter. These are commonly used in auto-body repair, sheet metal, plumbing, and electrical applications. Washers are also important for preventing corrosion, particularly by insulating steel screws from aluminum surfaces.
Advantages:
1. Good after sales service. Any small problem happening will be solved at the most prompt time;
2. Many years of export experience;
3. Specifications list is available upon your request
4. Welcome to send enquiry, we will reply soon.
5. Prompt shipment with professional documents
6. Custom packing, with photo before shipment
7. High quality and competitive price.
Company Details
Business Type:
Manufacturer,Trading Company
Year Established:
2004
Total Annual:
2000000-3000000
Employee Number:
100~200
Ecer Certification:
Active Member
Haiyan Juxing Trading Co., Ltd (Haiyan Julong) is a specialist engaged in fastener production, trade in services integrated enterprise, the company relies on abundant capital strength, the scale of production, perfect marketing network and quality service, has won the praise of customers a... Haiyan Juxing Trading Co., Ltd (Haiyan Julong) is a specialist engaged in fastener production, trade in services integrated enterprise, the company relies on abundant capital strength, the scale of production, perfect marketing network and quality service, has won the praise of customers a...
Get in touch with us
Leave a Message, we will call you back quickly!